Skip to content
ASTM A213/ASME SA213 T92pipesfactory2018-11-13T10:31:40+00:00ASTM A213/ASME SA213 Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater and Heat-Exchanger Tubes
Chemical Composition of ASTM A213 T92 Alloy Steel Pipes
| C % | Mn % | P % | S % | Si % | Cr % | Mo % | V % | N % | Ni % | Al % | Nb % | W % | B % |
| 0.07-0.13 | 0.3-0.6 | 0.02 max | 0.01 max | 0.5 max | 8.5-9.5 | 0.3-0.6 | 0.15-0.25 | 0.03-0.07 | 0.4 max | 0.04 max | 0.04-0.09 | 1.5-2.0 | 0.001-0.006 |
Mechanical Properties of ASTM A213 T92 Alloy Steel Pipes
| Tensile Strength, Mpa | Yield Strength, MPa | Elongation, % | Hardness, HB |
| 620 min | 440 min | 20 min | 250 max |
Page load link