Skip to content
ASTM A213/ASME SA213 T2pipesfactory2018-11-13T04:52:03+00:00ASTM A213/ASME SA213 Standard Specification for Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Chemical Composition of ASTM A213 T2 Alloy Steel Pipes
| C % | Mn % | P % | S % | Si % | Cr % | Mo % |
| 0.10-0.20 | 0.30-0.61 | 0.025 max | 0.025 max | 0.10-0.30 | 0.50-0.81 | 0.44-0.65 |
Mechanical Properties of ASTM A213 T2 Alloy Steel Pipes
| Tensile Strength, Mpa | Yield Strength, MPa | Elongation, % | Hardness, HB |
| 415 min | 205 min | 30 min | 163 max |